Ingot
형태 : Mo-Shield류
순도 : 99.95%
규격 : 협의
| Mesh & Weave | Rod | Sheet | |
|---|---|---|---|
| MO | 1800 | 1600 | 1600 |
| Ta | 2300 | - | 2300 |
| W(short term) | 3000 | 3000 | - |
| W(maximum time) | 2450 | 2450 | - |
| W | MO | |
|---|---|---|
| Dry H2 | no reaction | |
| Dry N3 | no reaction | |
| NH3 | 1000℃ dry gas: no reaction | |
| Air | 500℃ | 400℃ |
| Water vapor | Dew points between 10℃ and 20 ℃ : 1370℃ At lower points : no reaction | |
| CO | 1400℃ | 1400℃ |
| CO2 | 1200℃ | 1240℃ |
| Hydro carbon | 1200℃ | 1100℃ |
| VAC | 2500℃ | 1800℃ |
| in vacuum | ||
|---|---|---|
| W | MO | |
| Aluminum oxide | 1900℃ | 1900℃ |
| Beryllium oxide | 2000℃ | 1900℃ |
| Graphite | 1200℃ | 1100℃ |
| Magnetite oxide | 1600℃ | 1600℃ |
| Silicon carbons | 1300℃ | 1300℃ |
| Zirconium oxide | 1900℃ | 1900℃ |